Finishing Area

Used to refinish weapons via Fast Rust or Slow Rust process.

Current project is to restore a Smith & Wesson 38 Special and a Supermatic Citation in 22LR.

Current setup for rust bluing.

IMG_2768.HEIC

Using distilled water to heat up and rust the parts.

IMG_2767.HEIC

Hanging the parts in the cabinet induces rust on the parts.  Notice the Humidity and Temperature level.

IMG_2766.HEIC

After repeated rust applications and removal the finish starts to stick.